Recovery of scandium from silicate minerals by high …
A silicate concentrate ore has the Sc content of 1.03 × 10 −4 wt%, whose main minerals are limonite, chlorite, sericite, and hornblende, in the primary occurrence of isomorphism. (2) The leaching efficiency of Sc can reach 91.82% in pressure of 5.0 × 10 5 Pa, with A/O value of 1.1, L/S value of 1.8, 2 wt% dosage of NaF, at 130 °C for 6 h.